# Grade 2205 duplex

Global Stainless Steel, Nigel, Gauteng

High-strength duplex for chloride service. Listed pending DUPLEX_GRADES.

Stocked grade.

Also called: 1.4462, duplex, UNS S31803
Designations: Alloy 2205 / ASTM A240; UNS S32205; EN 1.4462 (X2CrNiMoN22-5-3)
Specifications: ASTM A240, ASTM A276, EN 10088-2, NACE MR0175
Standards: EN 10088-2, ASTM A240
Used for: chemical tanks, marine shafts
Typical products: Offshore oil and gas flowlines, subsea manifolds, and risers, Chemical cargo tanks and maritime chemical tankers, Desalination high-pressure reverse osmosis (RO) piping and pumps, Pulp and paper digesters and bleaching scrubbers
Industries: Offshore Oil & Gas, Desalination, Marine Cargo, Pulp & Paper, Chemical Processing

## Composition (as specified)

- Iron (Fe): Balance
- Carbon (C): max 0.030%
- Chromium (Cr): 22.00-23.00%
- Nickel (Ni): 4.50-6.50%
- Molybdenum (Mo): 3.00-3.50%
- Nitrogen (N): 0.14-0.20%
- Manganese (Mn): max 2.00%
- Silicon (Si): max 1.00%
- Phosphorus (P): max 0.030%
- Sulfur (S): max 0.020%

## PREN

Window 34.14 to 37.75 from the standard's composition limits (Cr + 3.3 Mo + 16 N); nominal 35.95.

## Mechanical properties (indicative)

- Tensile strength: 655 MPa / 95 ksi
- Yield strength: 450 MPa / 65.3 ksi
- Elongation at break: 25%
- Hardness: 260 HBW / 100 HRB
- Modulus of elasticity: 200 GPa / 29 Mpsi
- Density: 7.8 g/cm³ / 0.282 lb/in³
- Thermal conductivity: 19 W/(m·K) / 131.7 BTU·in/(hr·ft²·°F)
- Thermal expansion: 13 µm/(m·K) / 7.2 µin/(in·°F)

The source does not state the test condition these were measured in; ask for the mill certificate.

## Service notes

- Chloride exposure: Superb resistance to chloride stress corrosion cracking (SCC) and localized pitting in marine and brackish waters.
- Acidic exposure: High resistance to wet sulfuric, phosphoric, and organic acids, and hydrogen sulfide (H2S sour service).
- Sensitisation: Excellent; duplex microstructural balance (50% ferrite / 50% austenite) retards intergranular corrosion; vulnerable to 475°C embrittlement and sigma phase precipitation between 600°C–900°C.
- Weldability: Very Good; requires controlled heat input and over-alloyed filler metal (e.g., 2209) to preserve 50:50 phase ratio and nitrogen retention.
- Formability: Moderate; higher yield strength requires double the forming power of 304 and displays higher springback.
- Machinability index: 40% of AISI 1212

Disclaimer: The specifications and data on this site are provided for general information only. Verify any real-world project with a qualified metallurgist before relying on these figures. We take no responsibility for the use and application of this information.

Request a quote: https://globalstainless.direct/grades/2205/