# Grade 304L

Global Stainless Steel, Nigel, Gauteng

Low-carbon 304 for heavier welded sections.

Stocked grade.

Also called: 1.4307, AISI 304L
Designations: AISI 304L / SAE 30304L; UNS S30403; EN 1.4307 (X2CrNi18-9)
Specifications: ASTM A240, ASTM A276, EN 10088-2
Standards: EN 10088-2, ASTM A240
Used for: welded tanks, food plant
Typical products: Welded chemical reaction vessels and piping, Brewery fermentation tanks and distillation columns, Cryogenic storage tanks and vacuum insulated containers, Mining and wastewater processing fluid systems
Industries: Chemical Processing, Brewing & Distilling, Cryogenics, Wastewater Treatment

## Composition (as specified)

- Iron (Fe): Balance
- Carbon (C): max 0.030%
- Chromium (Cr): 17.50-19.50%
- Nickel (Ni): 8.00-12.00%
- Manganese (Mn): max 2.00%
- Silicon (Si): max 0.75%
- Nitrogen (N): max 0.10%
- Phosphorus (P): max 0.045%
- Sulfur (S): max 0.030%

## PREN

Window 17.5 to 21.1 from the standard's composition limits (Cr + 3.3 Mo + 16 N); nominal 19.3.

## Mechanical properties (indicative)

- Tensile strength: 485 MPa / 70.3 ksi
- Yield strength: 170 MPa / 24.7 ksi
- Elongation at break: 40%
- Hardness: 160 HBW / 85 HRB
- Modulus of elasticity: 193 GPa / 28 Mpsi
- Density: 8 g/cm³ / 0.289 lb/in³
- Thermal conductivity: 16.2 W/(m·K) / 112.4 BTU·in/(hr·ft²·°F)
- Thermal expansion: 17.2 µm/(m·K) / 9.6 µin/(in·°F)

The source does not state the test condition these were measured in; ask for the mill certificate.

## Service notes

- Chloride exposure: Similar to 304; moderate resistance, prone to crevice/pitting in marine salt-spray without regular cleaning.
- Acidic exposure: Resistant to organic and oxidizing acids; immune to intergranular attack across weld heat-affected zones (HAZ).
- Sensitisation: Extremely high resistance due to low carbon (<=0.030%); eliminates need for post-weld solution annealing.
- Weldability: Superior (highest in standard austenitic family); minimal carbide precipitation during heavy-section welding.
- Formability: Excellent; low work hardening yield allows severe drawing, spin forming, and stamping.
- Machinability index: 45% of AISI 1212

## Carried in

- [Stainless steel sheet](https://globalstainless.direct/products/stainless-steel/sheet/)
- [Stainless steel plate](https://globalstainless.direct/products/stainless-steel/plate/)
- [Stainless steel round bar](https://globalstainless.direct/products/stainless-steel/round-bar/)
- [Stainless steel tube](https://globalstainless.direct/products/stainless-steel/tube/)

Disclaimer: The specifications and data on this site are provided for general information only. Verify any real-world project with a qualified metallurgist before relying on these figures. We take no responsibility for the use and application of this information.

Request a quote: https://globalstainless.direct/grades/304l/
Canonical: https://globalstainless.direct/grades/304l/