# Grade 316

Global Stainless Steel, Nigel, Gauteng

Molybdenum-bearing grade for better pitting and chemical resistance.

Stocked grade.

Also called: 1.4401, AISI 316
Designations: AISI 316 / SAE 30316; UNS S31600; EN 1.4401 (X5CrNiMo17-12-2)
Specifications: ASTM A240, ASTM A276, EN 10088-2
Standards: EN 10088-2, EN 10088-3, ASTM A240, ASTM A276
Used for: chemical plant, marine fittings, dairy
Typical products: Marine deck fittings, rigging, and fasteners, Chemical plant valve bodies and pump casings, Petrochemical heat exchangers and distillation trays, Industrial dyeing and textile processing machinery
Industries: Marine, Petrochemical, Chemical Processing, Textiles

## Composition (as specified)

- Iron (Fe): Balance
- Carbon (C): max 0.080%
- Chromium (Cr): 16.00-18.00%
- Nickel (Ni): 10.00-14.00%
- Molybdenum (Mo): 2.00-3.00%
- Manganese (Mn): max 2.00%
- Silicon (Si): max 0.75%
- Nitrogen (N): max 0.10%
- Phosphorus (P): max 0.045%
- Sulfur (S): max 0.030%

## PREN

Window 22.6 to 29.5 from the standard's composition limits (Cr + 3.3 Mo + 16 N); nominal 26.05.

## Mechanical properties (indicative)

- Tensile strength: 515 MPa / 74.7 ksi
- Yield strength: 205 MPa / 29.7 ksi
- Elongation at break: 40%
- Hardness: 175 HBW / 88 HRB
- Modulus of elasticity: 193 GPa / 28 Mpsi
- Density: 8 g/cm³ / 0.289 lb/in³
- Thermal conductivity: 16.3 W/(m·K) / 113.1 BTU·in/(hr·ft²·°F)
- Thermal expansion: 16 µm/(m·K) / 8.9 µin/(in·°F)

The source does not state the test condition these were measured in; ask for the mill certificate.

## Service notes

- Chloride exposure: High resistance to chlorides and pitting due to 2.0–3.0% Mo; withstands typical marine splash zones.
- Acidic exposure: Substantially higher resistance to dilute sulfuric acid, phosphoric acid, and acetic acid solutions than 304.
- Sensitisation: Susceptible to sensitization in weld HAZ if subjected to continuous service in 425°C–860°C range.
- Weldability: Very Good; standard fusion techniques applicable; filler metal typically AWS ER316 or ER316L.
- Formability: Very Good; slightly higher work-hardening rate than 304 due to Mo content.
- Machinability index: 40% of AISI 1212

## Carried in

- [Stainless steel sheet](https://globalstainless.direct/products/stainless-steel/sheet/)
- [Stainless steel plate](https://globalstainless.direct/products/stainless-steel/plate/)
- [Stainless steel tread plate](https://globalstainless.direct/products/stainless-steel/tread-plate/)
- [Stainless steel round bar](https://globalstainless.direct/products/stainless-steel/round-bar/)
- [Stainless steel flat bar](https://globalstainless.direct/products/stainless-steel/flat-bar/)
- [Stainless steel square bar](https://globalstainless.direct/products/stainless-steel/square-bar/)
- [Stainless steel angle](https://globalstainless.direct/products/stainless-steel/angle/)
- [Stainless steel channel](https://globalstainless.direct/products/stainless-steel/channel/)
- [Stainless steel tube](https://globalstainless.direct/products/stainless-steel/tube/)
- [Stainless steel pipe](https://globalstainless.direct/products/stainless-steel/pipe/)
- [Stainless steel fittings](https://globalstainless.direct/products/stainless-steel/fittings/)
- [Stainless steel flanges](https://globalstainless.direct/products/stainless-steel/flanges/)
- [Stainless steel hollow bar](https://globalstainless.direct/products/stainless-steel/hollow-bar/)
- [Stainless steel mesh](https://globalstainless.direct/products/stainless-steel/mesh/)
- [Stainless steel perforated sheet](https://globalstainless.direct/products/stainless-steel/perforated-sheet/)
- [Stainless steel hex bar](https://globalstainless.direct/products/stainless-steel/hex-bar/)

Disclaimer: The specifications and data on this site are provided for general information only. Verify any real-world project with a qualified metallurgist before relying on these figures. We take no responsibility for the use and application of this information.

Request a quote: https://globalstainless.direct/grades/316/
Canonical: https://globalstainless.direct/grades/316/