# Grade 316Ti

Global Stainless Steel, Nigel, Gauteng

Type 316Ti Titanium-Stabilized Stainless Steel, austenitic stainless steel.

Reference metallurgy - available on request, not a stocked grade.

Designations: AISI 316Ti / SAE 30316Ti; UNS S31635; EN 1.4571 (X6CrNiMoTi17-12-2)
Specifications: ASTM A240, EN 10088-2, DIN 17440
Typical products: Flue gas desulfurization (FGD) scrubber liners, High-temperature chemical processing reactors, Exhaust system components for heavy marine diesels, Nuclear engineering reprocessing piping
Industries: Petrochemical, Energy, Nuclear, Marine

## Composition (as specified)

- Iron (Fe): Balance
- Carbon (C): max 0.080%
- Chromium (Cr): 16.00-18.00%
- Nickel (Ni): 10.00-14.00%
- Molybdenum (Mo): 2.00-3.00%
- Titanium (Ti): 0.20-0.70%
- Manganese (Mn): max 2.00%
- Silicon (Si): max 0.75%
- Nitrogen (N): max 0.10%
- Phosphorus (P): max 0.045%
- Sulfur (S): max 0.030%

## PREN

Window 22.6 to 29.5 from the standard's composition limits (Cr + 3.3 Mo + 16 N); nominal 26.05.

## Mechanical properties (indicative)

- Tensile strength: 520 MPa / 75.4 ksi
- Yield strength: 215 MPa / 31.2 ksi
- Elongation at break: 35%
- Hardness: 180 HBW / 89 HRB
- Modulus of elasticity: 195 GPa / 28.3 Mpsi
- Density: 8 g/cm³ / 0.289 lb/in³
- Thermal conductivity: 16.3 W/(m·K) / 113.1 BTU·in/(hr·ft²·°F)
- Thermal expansion: 16.5 µm/(m·K) / 9.2 µin/(in·°F)

The source does not state the test condition these were measured in; ask for the mill certificate.

## Service notes

- Chloride exposure: Equivalent to 316 in marine chloride pitting resistance.
- Acidic exposure: Resistant to dilute sulfuric acid and organic acid vapors at elevated temperatures.
- Sensitisation: Stabilized with Titanium: preferentially forms TiC precipitates, preventing chromium depletion at grain boundaries up to 800°C.
- Weldability: Good; requires Ti-stabilized or low-carbon filler wire (ER316L / ER318) to avoid weld bloom.
- Formability: Moderate to Good; titanium carbonitride inclusions slightly reduce polishability and fine formability.
- Machinability index: 38% of AISI 1212

Disclaimer: The specifications and data on this site are provided for general information only. Verify any real-world project with a qualified metallurgist before relying on these figures. We take no responsibility for the use and application of this information.

Request a quote: https://globalstainless.direct/grades/316ti/
Canonical: https://globalstainless.direct/grades/316ti/