# Grade 430

Global Stainless Steel, Nigel, Gauteng

Type 430 Ferritic Stainless Steel (17% Chrome), ferritic stainless steel.

Reference metallurgy - available on request, not a stocked grade.

Designations: AISI 430 / SAE 51430; UNS S43000; EN 1.4016 (X6Cr17)
Specifications: ASTM A240, ASTM A276, EN 10088-2
Typical products: Dishwasher interior liners and clothes dryer drums, Refrigerator cabinet panels and appliance trims, Automotive decorative trim and wheel covers, Nitric acid plant absorber towers and storage tanks
Industries: Appliances, Automotive, Chemical Processing, Architecture (Interior)

## Composition (as specified)

- Iron (Fe): Balance
- Carbon (C): max 0.12%
- Chromium (Cr): 16.00-18.00%
- Nickel (Ni): max 0.75%
- Manganese (Mn): max 1.00%
- Silicon (Si): max 1.00%
- Phosphorus (P): max 0.040%
- Sulfur (S): max 0.030%

## PREN

Window 16 to 18 from the standard's composition limits (Cr + 3.3 Mo + 16 N); nominal 17.

## Mechanical properties (indicative)

- Tensile strength: 450 MPa / 65.3 ksi
- Yield strength: 260 MPa / 37.7 ksi
- Elongation at break: 22%
- Hardness: 160 HBW / 85 HRB
- Modulus of elasticity: 200 GPa / 29 Mpsi
- Density: 7.75 g/cm³ / 0.28 lb/in³
- Thermal conductivity: 26.1 W/(m·K) / 181 BTU·in/(hr·ft²·°F)
- Thermal expansion: 10.4 µm/(m·K) / 5.8 µin/(in·°F)

The source does not state the test condition these were measured in; ask for the mill certificate.

## Service notes

- Chloride exposure: Moderate atmospheric resistance; not recommended for outdoor marine exposure due to staining/pitting.
- Acidic exposure: Resistant to nitric acid (HNO3) and mild organic acids; widely used in chemical equipment handling nitric acid.
- Sensitisation: Susceptible to sensitization in weld HAZ due to grain boundary chromium carbide precipitation; requires post-weld annealing.
- Weldability: Fair; HAZ exhibits grain coarsening and room-temperature embrittlement; preheat to 150°C–200°C recommended.
- Formability: Good bending and roll forming; lower stretch formability than 304 due to lower work hardening coefficient.
- Machinability index: 55% of AISI 1212

Disclaimer: The specifications and data on this site are provided for general information only. Verify any real-world project with a qualified metallurgist before relying on these figures. We take no responsibility for the use and application of this information.

Request a quote: https://globalstainless.direct/grades/430/
Canonical: https://globalstainless.direct/grades/430/