Working numbers from the same validated data the data sheets use. Type a comma or a point decimal; both are read the same. Every result is indicative arithmetic, not a certification - the standard and the mill certificate decide.

PREN diagram: passive chromium-molybdenum-nitrogen oxide film arresting chloride pitting attack, weighting Cr by 1, Mo by 3,3 and N by 16 to reach PREN 35,4 on the 0 to 50 service-environment ladder.%Cr + 3,3 × %Mo + 16 × %NPREN 35,4Aqueous chloride (Cl⁻)Passive oxide barrierCl⁻Cl⁻Cl⁻Cl⁻Cr → Cr₂O₃ filmMo → pit arrestN → buffer pHElemental weightingIndex pointsCr22% × 1+22Mo3,2% × 3,3+10,6N0,18% × 16+2,935,4 (Seawater)FreshwaterBrackishSeawaterOffshore020324050

Pitting resistance (PREN)

Type a chemistry in weight percent; the score sits on the service-environment ladder and points at the grades whose specified windows contain it.

Nitrogen weighting

The 16× form is the common one; super duplex houses often weight nitrogen at 30. The choice is yours to make, so it is a control, not an assumption.

PREN = %Cr + 3,3 × %Mo + 16 × %N

Unit conversion diagram for strength: an invariant physical specimen measured simultaneously on a metric MPa scale and an imperial ksi scale via factor 0,15.StrengthMPa → ksiMetric (SI): MPaImperial: ksiOne physical state across both measurement scales515 MPa0–1 000 MPa74,69 ksi0–145 ksi× 0,1450 ↓Data-table quantitiesExact factorStrengthMPa ↔ ksiModulusGPa ↔ MpsiDensityg/cm³ ↔ lb/in³ThermalW/m·K ↔ BTUExpan.µm/K ↔ µin/°F

Unit conversion

Only the quantities the data tables carry, with the same conversion factors - nothing here invents precision the source does not have.

Result in ksi

Section weight diagram: 2D cross-section (Ø25 mm, area 491 mm²) extruded across length 6 m at density 8 g/cm³ for a theoretical mass of 23,6 kg.Area × Length × Density23,6 kg (3,93 kg/m)1. Cross-section (A)2. Extruded length (L × ρ)Ø25 mmA = 491 mm²304 (8 g/cm³)L = 6 mRound (Ø)SquareHex (AF)PlateVolumetric mass chain (mm² × m × g/cm³ ÷ 1 000)Area (A)491 mm²×Length (L)6 m×Density (ρ)8 g/cm³=Mass (m)23,6 kg

Section weight

Theoretical mass from the alloy's stated density. Mill tolerance and the actual heat decide the delivered weight - use this to size a quote, not to certify a lift.

Enter the dimensions to see the mass.

PREN is a screening index, not a corrosion guarantee; the formula used is stated beside the result. Weights are theoretical from the alloy's stated density - mill tolerance decides the delivered figure. For a real number against real stock, request a quote.

The specifications and data on this site are provided for general information only. Verify any real-world project with a qualified metallurgist before relying on these figures. We take no responsibility for the use and application of this information.